Author Topic: Refinishing/Customizing a Method  (Read 3095 times)

golferoz

  • Newbie
  • *
  • Posts: 33
Refinishing/Customizing a Method
« on: June 28, 2010, 11:45:18 AM »
Anyone here done any customizing with their Method?  Paintfill stuff looks pretty simple, but I am wondering about BOS refinishing or a white ploymer type thing.  Don't know if there is a heat treatment to those things...which would melt the poly inserts in the face of the Method.  If the finishes are dipped, then maybe the grooves could be masked off?  Any suggestions would be appreciated.

putterplating

  • Section Moderator
  • Hero Member
  • *****
  • Posts: 1760
  • Look who got their putter refinished!
    • Colbert Putter Plating
Re: Refinishing/Customizing a Method
« Reply #1 on: July 13, 2010, 08:10:44 PM »
It is a combination of stainless steel & tungsten.  So, the stainless portion could be done in a darker finish.  The polymer would not be ruined.